Abstract

Electrical discharge machining of conducting ceramics is often associated with high roughness and porosity, which hinders their application. This porosity-laden surface morphology necessitates a postprocessing technique to reduce the severity of the surface defects. Hence, this study focuses on the utilization of a nanosecond pulsed laser as a surface modification tool to minimize the debris and pores formed on the surface after the wire-electrical discharge machining process. This paper presents a study on the influence of laser parameters, viz., power, number of scans, scanning speed, and pulse repetition rate on the overall surface characteristics. The concentration of surface debris and pores were observed to significantly decrease with laser surface modification (LSM). The improvement in the surface characteristics after laser processing with low fluence was mainly attributed to melting, vaporization, and subsequent flow of molten material, which led to filling of the surface pores. This resulted in a more even surface postlaser surface modification. The surface roughness was observed to decrease by ∼49% after the laser processing at lower values of laser power, number of scans, and scanning speed and at higher values of pulse repetition rate. Furthermore, spatial, hybrid, and functional volume characteristics were observed to improve postlaser modification. However, at higher laser fluence, the processed surfaces were observed to get further worsened with the formation of deep ridges.

References

1.
Singh
,
M. A.
,
Sarma
,
D. K.
,
Hanzel
,
O.
,
Sedlacek
,
J.
, and
Sajgalik
,
P.
,
2017
, “
Machinability Analysis of Multi Walled Carbon Nanotubes Filled Alumina Composites in Wire Electrical Discharge Machining Process
,”
J. Eur. Ceram. Soc.
,
37
, pp.
3107
3114
.10.1016/j.jeurceramsoc.2017.03.058
2.
Melk
,
L.
,
Antti
,
M. L.
, and
Anglada
,
M.
,
2016
, “
Material Removal Mechanism by EDM of Zirconia Reinforced MWCNT Nanocomposites
,”
Ceram. Int.
,
42
, pp.
5792
5801
.10.1016/j.ceramint.2015.12.120
3.
Hanzel
,
O.
,
Singh
,
M. A.
,
Marla
,
D.
,
Sedlak
,
R.
, and
Sajgalik
,
P.
,
2019
, “
Wire Electrical Discharge Machinable SiC With GNPs and GO as the Electrically Conducting Filler
,”
J. Eur. Ceram. Soc.
,
39
, pp.
2626
2633
.10.1016/j.jeurceramsoc.2019.03.012
4.
Satyarthi
,
M.
, and
Pandey
,
P. M.
,
2013
, “
Comparison of EDG, Diamond Grinding and EDM Processing of Conductive Alumina Ceramics Composite
,”
Mater. Manuf. Process.
,
28
, pp.
369
374
.10.1080/10426914.2012.736663
5.
Singh
,
M. A.
,
Sarma
,
D. K.
,
Hanzel
,
O.
,
Sedlacek
,
J.
, and
Sajgalik
,
P.
,
2018
, “
Surface Characteristics Enhancement of MWCNT Alumina Composites Using Multi-Pass WEDM Process
,”
J. Eur. Ceram. Soc.
,
38
, pp.
4035
4042
.10.1016/j.jeurceramsoc.2018.04.062
6.
Mandal
,
A.
,
Dixit
,
A. R.
,
Chattopadhyaya
,
S.
,
Paramanik
,
A.
,
Hloch
,
S.
, and
Krolczyk
,
G.
,
2017
, “
Improvement of Surface Integrity of Nimonic C 263 Super Alloy Produced by WEDM Through Various Post-Processing Techniques
,”
Int. J. Adv. Manuf. Technol.
,
93
, pp.
433
443
.10.1007/s00170-017-9993-x
7.
Wang
,
C. C.
,
Chow
,
H. M.
,
Yang
,
L. D.
, and
Lu
,
C. T.
,
2009
, “
Recast Layer Removal After Electrical Discharge Machining Via Taguchi Analysis: A Feasibility Study
,”
J. Mater. Process. Technol.
,
209
, pp.
4134
4140
.10.1016/j.jmatprotec.2008.10.012
8.
Hsu
,
H. Y.
, and
Hu
,
C. C.
,
2017
, “
Surface Quality Improvement of EDMed Ti-6Al-4V Alloy Using Plasma Etching and TiN Coating
,”
Int. J. Adv. Manuf. Technol.
,
88
, pp.
67
74
.10.1007/s00170-016-8760-8
9.
Pfefferkorn
,
P.
,
Duffie
,
N. A.
,
Morrow
,
J. D.
, and
Wang
,
Q.
,
2014
, “
Effect of Beam Diameter on Pulsed Laser Polishing of S7 Tool Steel
,”
CIRP Ann. Manuf. Technol.
,
63
, pp.
237
240
.10.1016/j.cirp.2014.03.055
10.
Marimuthu
,
S.
,
Triantaphyllou
,
A.
,
Antar
,
M.
,
Wimpenny
,
D.
, and
Morton
,
H.
,
2015
, “
Laser Polishing of Selective Laser Melted Components
,”
Int. J. Mach. Tool Manuf.
,
95
, pp.
97
104
.10.1016/j.ijmachtools.2015.05.002
11.
Palomar
,
T.
,
Oujja
,
M.
,
Llorente
,
I.
,
Barat
,
B. R.
,
Canamares
,
M. V.
, and
Cano
,
E.
,
2016
, “
Evaluation of Laser Cleaning for the Restoration of Tarnished Silver Artefacts
,”
Appl. Surf. Sci.
,
387
, pp.
118
127
.10.1016/j.apsusc.2016.06.017
12.
Walder
,
G.
, and
Richard
,
J.
,
2016
, “
Removal of the Heat Affect Zone Created by EDM With Pico-Second LASER Machining
,”
Proc. CIRP.
,
42
, pp.
475
480
.10.1016/j.procir.2016.02.235
13.
Haupt
,
S.
,
Schmidt
,
J.
, and
Fleischer
,
J.
,
2006
, “
Post Processing of EDM-Machined Microstructures by Ultra Short Pulsed Laser Ablation
,”
International Congress on Laser Materials Processing and Laser Microfabrication
, 2006, pp.
174
178
.
14.
Marla
,
D.
,
Bhandarkar
,
U.
, and
Joshi
,
S.
,
2013
, “
A Model of Laser Ablation With Temperature-Dependent Material Properties, Vaporization, Phase Explosion
,”
Appl. Phys. A-Mater.
,
116
, pp.
273
285
.10.1007/s00339-013-8118-0
15.
Xing
,
Y.
,
Liu
,
L.
,
Wu
,
Z.
,
Wang
,
X.
,
Huang
,
P.
, and
Tang
,
L.
,
2018
, “
Fabrication and Characterization of Micro-Channels on Al2O3/TiC Ceramic Produced by Nanosecond Laser
,”
Ceram. Int.
,
44
, pp.
23035
23044
.10.1016/j.ceramint.2018.09.106
You do not currently have access to this content.