Stress whitening problem in thermoformed alumina trihydrate (ATH) reinforced poly(methyl methacrylate) (PMMA) was studied. In situ heavy-gage thermoforming of acrylics was entirely replicated under laboratory controlled conditions at different operation parameters. Samples were monitored with optical microscope after the completion of the thermoforming operation. For stress whitening quantification, a new index was proposed from image histograms of processed optical micrographs. Results indicated that stress whitening in PMMA/ATH samples increases with level of plastic deformation at all thermoforming conditions. The influence of the forming rate and forming temperature on the degree of stress whitening was explained in terms of change in material behavior and microdeformation mechanisms around two characteristic temperatures of PMMA/ATH. Developed method for stress whitening quantification characterizes different levels of stress whitening with single numeric values. It is shown that stress whitening index and density of microdeformation features display a strong correlation. Higher density of particle cracks at low forming temperatures results in higher stress whitening levels. Increased surface irregularity and large size voids at high forming temperatures produce lower stress whitening.

1.
Throne
,
J. L.
, 1996,
Technology of Thermoforming
,
Hanser Publishers
,
New York
.
2.
Rosato
,
D. V.
, 2002,
Plastics Institute of America Plastics Engineering, Manufacturing and Data Handbook
,
Kluwer
,
Dordrecht
.
3.
Nathani
,
H.
,
Dasari
,
A.
, and
Misra
,
R. D. K.
, 2004, “
On the Reduced Susceptibility to Stress Whitening Behavior of Melt Intercalated Polybutene-Clay Nanocomposites During Tensile Straining
,”
Acta Mater.
1359-6454,
52
, pp.
3217
3227
.
4.
Pae
,
K. D.
,
Chu
,
H. C.
,
Lee
,
J. K.
, and
Kim
,
J. H.
, 2000, “
Healing of Stress-Whitening in Polyethylene and Polypropylene at or Below Room Temperature
,”
Polym. Eng. Sci.
0032-3888,
40
, pp.
1783
1795
.
5.
Tanniru
,
M.
, and
Misra
,
R. D. K.
, 2006, “
Reduced Susceptibility to Stress Whitening During Tensile Deformation of Calcium Carbonate-Reinforced High Density Polyethylene Composites
,”
Mater. Sci. Eng., A
0921-5093,
424
, pp.
53
70
.
6.
Chandavasu
,
C.
,
Xanthos
,
M.
,
Sirkar
,
K. K.
, and
Gogos
,
C. G.
, 2000, “
Preparation of Microporous Films From Immiscible Blends via Melt Processing
,”
J. Plast. Film Sheeting
8756-0879,
16
(
4
), pp.
288
300
.
7.
Dasari
,
A.
, and
Misra
,
R. D. K.
, 2004, “
The Role of Micrometric Wollastonite Particles on Stress Whitening Behavior of Polypropylene Composites
,”
Acta Mater.
1359-6454,
52
, pp.
1683
1697
.
8.
Liu
,
Y.
,
Kennard
,
C. H. L.
,
Truss
,
R. W.
, and
Calos
,
N. J.
, 1997, “
Characterization of Stress-Whitening of Tensile Yielded Isotactic Polypropylene
,”
Polymer
0032-3861,
38
, pp.
2797
2805
.
9.
Thridandapani
,
R. R.
,
Mudaliar
,
A.
,
Yuan
,
Q.
, and
Misra
,
R. D. K.
, 2006, “
Near Surface Deformation Associated With the Scratch in Polypropylene-Clay Nanocomposite: A Microscopic Study
,”
Mater. Sci. Eng., A
0921-5093,
418
, pp.
292
302
.
10.
Dasari
,
A.
, and
Misra
,
R. D. K.
, 2004, “
Microscopic Aspects of Surface Deformation and Fracture of High Density Polyethylene
,”
Mater. Sci. Eng., A
0921-5093,
367
, pp.
248
260
.
11.
Mudaliar
,
A.
,
Yuan
,
Q.
, and
Misra
,
R. D. K.
, 2006, “
On Surface Deformation of Melt-Intercalated Polyethylene-Clay Nanocomposites During Scratching
,”
Polym. Eng. Sci.
0032-3888,
46
, pp.
1625
1634
.
12.
Misra
,
R. D. K.
,
Nathani
,
H.
,
Dasari
,
A.
,
Wanjale
,
S. D.
, and
Jog
,
J. P.
, 2004, “
The Determining Role of Clay Particles on Mechanically Induced Surface Damage and Associated Stress Whitening in Polybutene-Clay Nanocomposites
,”
Mater. Sci. Eng., A
0921-5093,
386
, pp.
175
185
.
13.
Hadal
,
R.
,
Yuan
,
Q.
,
Jog
,
J. P.
, and
Misra
,
R. D. K.
, 2006, “
On Stress Whitening During Surface Deformation in Clay-Containing Polymer Nanocomposites: A Microstructural Approach
,”
Mater. Sci. Eng., A
0921-5093,
418
, pp.
268
281
.
14.
Tillier
,
D. L.
,
Meuldijk
,
J.
,
Höhne
,
G. W. H.
,
Frederik
,
P. M.
,
Regev
,
O.
, and
Koning
,
C. E.
, 2005, “
About Morphology in Ethylene-Propylene(-Diene) Copolymers-Based Latexes
,”
Polymer
0032-3861,
46
, pp.
7094
7108
.
15.
Lalande
,
L.
,
Plummer
,
C. J. G.
,
Manson
,
J. -A. E.
, and
Gérard
,
P.
, 2006, “
Microdeformation Mechanisms in Rubber Toughened PMMA and PMMA-Based Copolymers
,”
Eng. Fract. Mech.
0013-7944,
73
, pp.
2413
2426
.
16.
Mina
,
M. F.
,
Chowdhury
,
M. N. K.
,
Alam
,
A. K. M. M.
, and
Michler
,
G. H.
, 2006, “
Studies of Micromechanical Deformation Processes in Particle-Filled Glassy Polymer
,”
Polym.-Plast. Technol. Eng.
0360-2559,
45
, pp.
217
222
.
17.
Cho
,
K.
,
Yang
,
J.
, and
Park
,
C. E.
, 1998, “
The Effect of Rubber Particle Size on Toughening Behaviour of Rubber-Modified Poly(Methyl Methacrylate) With Different Test Methods
,”
Polymer
0032-3861,
39
, pp.
3073
3081
.
18.
Lalande
,
L.
,
Plummer
,
C. J. G.
,
Månson
,
J. -A. E.
, and
Gérard
,
P.
, 2006, “
The Influence of Matrix Modification on Fracture Mechanisms in Rubber Toughened Polymethylmethacrylate
,”
Polymer
0032-3861,
47
, pp.
2389
2401
.
19.
Plummer
,
C. J. G.
,
Béguelin
,
P.
, and
Kausch
,
H. H.
, 1999, “
Microdeformation in Core-Shell Particle Modified Polymethylmethacrylates
,”
Colloids Surf., A
0927-7757,
153
(
1–3
), pp.
551
566
.
20.
Misra
,
R. D. K.
,
Hadal
,
R.
, and
Duncan
,
S. J.
, 2004, “
Surface Damage Behavior During Scratch Deformation of Mineral Reinforced Polymer Composites
,”
Acta Mater.
1359-6454,
52
, pp.
4363
4376
.
21.
Tanniru
,
M.
,
Misra
,
R. D. K.
,
Berbrand
,
K.
, and
Murphy
,
D.
, 2005, “
The Determining Role of Calcium Carbonate on Surface Deformation During Scratching of Calcium Carbonate-Reinforced Polyethylene Composites
,”
Mater. Sci. Eng., A
0921-5093,
404
, pp.
208
220
.
22.
Dasari
,
A.
,
Rohrmann
,
J.
, and
Misra
,
R. D. K.
, 2003, “
Surface Microstructural Modification and Fracture Behavior of Tensile Deformed Polypropylene With Different Percentage Crystallinity
,”
Mater. Sci. Eng., A
0921-5093,
360
, pp.
237
248
.
23.
Dasari
,
A.
,
Rohrmann
,
J.
, and
Misra
,
R. D. K.
, 2003, “
Microstructural Aspects of Surface Deformation Processes and Fracture of Tensile Strained High Isotactic Polypropylene
,”
Mater. Sci. Eng., A
0921-5093,
358
, pp.
372
383
.
24.
Dasari
,
A.
,
Rohrmann
,
J.
, and
Misra
,
R. D. K.
, 2003, “
Microstructural Evolution During Tensile Deformation of Polypropylenes
,”
Mater. Sci. Eng., A
0921-5093,
351
, pp.
200
213
.
25.
Dasari
,
A.
, and
Misra
,
R. D. K.
, 2003, “
On the Strain Rate Sensitivity of High Density Polyethylene and Polypropylenes
,”
Mater. Sci. Eng., A
0921-5093,
358
, pp.
356
371
.
26.
Bucknall
,
C. B.
, 2001, “
Applications of Microscopy to the Deformation and Fracture of Rubber-Toughened Polymers
,”
J. Microsc.
0022-2720,
201
, pp.
221
229
.
27.
Petrich
,
R. P.
, 1973, “
Impact Reinforcement of Poly(Vinyl Chloride)
,”
Polym. Eng. Sci.
0032-3888,
13
, pp.
248
254
.
28.
Ma
,
X.
,
Sauer
,
J. A.
, and
Hara
,
M.
, 1995, “
Poly(Methyl Methacrylate) Based Ionomers. 1. Dynamic Mechanical Properties and Morphology
,”
Macromolecules
0024-9297,
28
(
11
), pp.
3953
3962
.
29.
Ma
,
X.
,
Sauer
,
J. A.
, and
Hara
,
M.
, 1995, “
Poly(Methyl Methacrylate) Ionomers. 2. Deformation Modes under Simple Tension
,”
Macromolecules
0024-9297,
28
(
16
), pp.
5526
5534
.
30.
Yuan
,
Q.
,
Ramisetti
,
N.
, and
Misra
,
R. D. K.
, 2008, “
Nanoscale Near-Surface Deformation in Polymer Nanocomposites
,”
Acta Mater.
1359-6454,
56
(
9
), pp.
2089
2100
.
31.
Dasari
,
A.
,
Misra
,
R. D. K.
, and
Rohrman
,
J.
, 2004, “
Scratch Deformation Characteristics of Micrometric Wollastonite-Reinforced Ethylene-Propylene Copolymer Composites
,”
Polym. Eng. Sci.
0032-3888,
44
, pp.
1738
1748
.
32.
Xiang
,
C.
,
Sue
,
H. J.
,
Chu
,
J.
, and
Masuda
,
K.
, 2001, “
Roles of Additives in Scratch Resistance of High Crystallinity Polypropylene Copolymers
,”
Polym. Eng. Sci.
0032-3888,
41
, pp.
23
31
.
33.
Bensason
,
S.
,
Hiltner
,
A.
, and
Baer
,
E.
, 1997, “
Damage Zone in PVC and PVC/MBS Blends. I. The Effect of Rubber Content and Temperature
,”
J. Appl. Polym. Sci.
0021-8995,
63
, pp.
703
713
.
34.
Gao
,
G.
,
Zhang
,
J.
,
Yang
,
H.
,
Zhou
,
C.
, and
Zhang
,
H.
, 2006, “
Deformation Mechanism of Polystyrene Toughened With Sub-Micrometer Monodisperse Rubber Particles
,”
Polym. Int.
0959-8103,
55
, pp.
1215
1221
.
35.
Gensler
,
R.
,
Plummer
,
C. J. G.
,
Grein
,
C.
, and
Kausch
,
H. H.
, 2000, “
Influence of the Loading Rate on the Fracture Resistance of Isotactic Polypropylene and Impact Modified Isotactic Polypropylene
,”
Polymer
0032-3861,
41
, pp.
3809
3819
.
36.
Dasari
,
A.
,
Yu
,
Z. -Z.
,
Yang
,
M.
,
Zhang
,
Q. -X.
,
Xie
,
X. -L.
, and
Mai
,
Y. -W.
, 2006, “
Micro- and Nano-Scale Deformation Behavior of Nylon 66-Based Binary and Ternary Nanocomposites
,”
Compos. Sci. Technol.
0266-3538,
66
, pp.
3097
3114
.
37.
Liu
,
J.
,
Sue
,
H. -J.
,
Thompson
,
Z. J.
,
Bates
,
F. S.
,
Dettloff
,
M.
,
Jacob
,
G.
,
Verghese
,
N.
, and
Pham
,
H.
, 2009, “
Strain Rate Effect on Toughening of Nano-Sized Pep-Peo Block Copolymer Modified Epoxy
,”
Acta Mater.
1359-6454,
57
(
9
), pp.
2691
2701
.
38.
Liu
,
Z.
,
Zhu
,
X.
,
Wu
,
L.
,
Li
,
Y.
,
Qi
,
Z.
,
Choy
,
C.
, and
Wang
,
F.
, 2001, “
Effects of Interfacial Adhesion on the Rubber Toughening of Poly(Vinyl Chloride) Part 1. Impact Tests
,”
Polymer
0032-3861,
42
, pp.
737
746
.
39.
Li
,
Z. -M.
,
Qian
,
Z. -Q.
,
Yang
,
M. -B.
,
Yang
,
W.
,
Xie
,
B. -H.
, and
Huang
,
R.
, 2005, “
Anisotropic Microstructure-Impact Fracture Behavior Relationship of Polycarbonate/Polyethylene Blends Injection-Molded at Different Temperatures
,”
Polymer
0032-3861,
46
, pp.
10466
10477
.
40.
Lazzeri
,
A.
,
Zebarjad
,
S. M.
,
Pracella
,
M.
,
Cavalier
,
K.
, and
Rosa
,
R.
, 2005, “
Filler Toughening of Plastics. Part 1–the Effect of Surface Interactions on Physico-Mechanical Properties and Rheological Behaviour of Ultrafine CaCo3/HDPE Nanocomposites
,”
Polymer
0032-3861,
46
, pp.
827
844
.
41.
Kody
,
R. S.
, and
Martin
,
D. C.
, 1996, “
Quantitative Characterization of Surface Deformation in Polymer Composites Using Digital Image Analysis
,”
Polym. Eng. Sci.
0032-3888,
36
, pp.
298
304
.
42.
Wong
,
M.
,
Moyse
,
A.
,
Lee
,
F.
, and
Sue
,
H. J.
, 2004, “
Study of Surface Damage of Polypropylene Under Progressive Loading
,”
J. Mater. Sci.
0022-2461,
39
, pp.
3293
3308
.
43.
Hornsby
,
P.
, and
Premphet
,
K.
, 1997, “
Fracture Toughness of Multiphase Polypropylene Composites Containing Rubbery and Particulate Inclusions
,”
J. Mater. Sci.
0022-2461,
32
, pp.
4767
4775
.
44.
Lee
,
C. -B.
, and
Chang
,
F. -C.
, 1992, “
Toughening Behavior of Elastomer-Modified Polycarbonates Based on the J-Integral
,”
Polym. Eng. Sci.
0032-3888,
32
, pp.
792
803
.
45.
Li
,
Q. -G.
,
Xie
,
B. -H.
,
Yang
,
W.
,
Li
,
Z. -M.
,
Zhang
,
W. -Q.
, and
Yang
,
M. -B.
, 2007, “
Effect of Annealing on Fracture Behavior of Poly(Propylene-Block-Ethylene) Using Essential Work of Fracture Analysis
,”
J. Appl. Polym. Sci.
0021-8995,
103
, pp.
3438
3446
.
46.
Ferrer-Balas
,
D.
,
Maspoch
,
M. L.
,
Martinez
,
A. B.
,
Ching
,
E.
,
Li
,
R. K. Y.
, and
Mai
,
Y. W.
, 2001, “
Fracture Behaviour of Polypropylene Films at Different Temperatures: Assessment of the EWF Parameters
,”
Polymer
0032-3861,
42
, pp.
2665
2674
.
47.
Ferrer-Balas
,
D.
,
Maspoch
,
M. L.
, and
Mai
,
Y. -W.
, 2002, “
Fracture Behaviour of Polypropylene Films at Different Temperatures: Fractography and Deformation Mechanisms Studied by SEM
,”
Polymer
0032-3861,
43
, pp.
3083
3091
.
48.
Gong
,
G.
,
Xie
,
B. -H.
,
Yang
,
W.
,
Li
,
Z. -M.
,
Lai
,
S. -M.
, and
Yang
,
M. -B.
, 2006, “
Plastic Deformation Behavior of Polypropylene/Calcium Carbonate Composites With and Without Maleic Anhydride Grafted Polypropylene Incorporated Using the Essential Work of Fracture Method
,”
Polym. Test.
0142-9418,
25
, pp.
98
106
.
49.
Lee
,
J. K.
,
Kim
,
J. H.
,
Kook
,
H. C. C.
, and
Pae
,
D.
, 2002, “
Macroscopic Observation of Healing Process in Stress-Whitened Polypropylene Under Hydrostatic Pressure
,”
Polym. Eng. Sci.
0032-3888,
42
, pp.
2351
2360
.
50.
Yamaguchi
,
M.
, and
Nitta
,
K. -H.
, 1999, “
Optical and Acoustical Investigation for Plastic Deformation of Isotactic Polypropylene/Ethylene-1-Hexene Copolymer Blends
,”
Polym. Eng. Sci.
0032-3888,
39
, pp.
833
840
.
51.
Kasajima
,
M.
,
Ito
,
K.
, and
Tsutsui
,
M.
, 1981, “
Influence of Temperature on Stress-Crazing of a Microcomposite Thermoplastic (Hips)
,”
J. Macromol. Sci., Phys.
0022-2348,
19
, pp.
649
664
.
52.
Kasajima
,
M.
,
Ito
,
K.
, and
Tsutsui
,
M.
, 1981, “
Relaxation Behavior of Stress-Crazing of a Microcomposite Thermoplastic (Hips)
,”
J. Macromol. Sci., Phys.
0022-2348,
19
, pp.
665
678
.
53.
Squire
,
M.
, 1997, “
Development of an Improved Stress Whitening Test Method for the Comparison of Polypropylene Impact Copolymers
,”
Proceedings of the ANTEC 1997 Plastics, Plastics Saving Planet Earth
, Vol.
3
, pp.
2771
2774
.
54.
Lee
,
C. D.
, 2005, “
Structure-Property Relations in Visbroken (Peroxide Treated) Impact Polypropylene Copolymers
,”
Proceedings of the ANTEC 2005 Plastics, Materials
, Vol.
2
, pp.
2035
2045
.
55.
1974, “
Use of Aluminum Trihydrate in a Poly Methyl Methacrylate Article
,” U.S. Patent No. 3,847,865.
56.
Basaran
,
C.
,
Nie
,
S.
,
Hutchins
,
C. S.
, and
Ergun
,
H.
, 2008, “
Influence of Interfacial Bond Strength on Fatigue Life and Thermo-Mechanical Behavior of a Particulate Composite: An Experimental Study
,”
Int. J. Damage Mech.
1056-7895,
17
(
2
), pp.
123
147
.
57.
Nie
,
S.
, 2005, “
A Micromechanical Study of the Damage Mechanics of Acrylic Particulate Composites Under Thermomechanical Loading
,” Ph.D. thesis, State University of New York at Buffalo, Buffalo.
58.
Morye
,
S. S.
, 2005, “
Comparison of the Thermoformability of a PPE/PP Blend With Thermoformable ABS. Part II: Large Deformation Methods
,”
Polym. Eng. Sci.
0032-3888,
45
, pp.
1377
1384
.
59.
Stephenson
,
M. J.
, and
Ryan
,
M. E.
, 1997, “
Experimental Study of the Thermoforming of a Blend of Styrene-Butadiene Copolymer With Polystyrene
,”
Polym. Eng. Sci.
0032-3888,
37
(
2
), pp.
450
459
.
60.
Dooling
,
P. J.
,
Buckley
,
C. P.
,
Rostami
,
S.
, and
Zahlan
,
N.
, 2002, “
Hot-Drawing of Poly(Methyl Methacrylate) and Simulation Using a Glass-Rubber Constitutive Model
,”
Polymer
0032-3861,
43
, pp.
2451
2465
.
61.
Münstedt
,
H.
,
Kurzbeck
,
S.
, and
Stange
,
J.
, 2006, “
Importance of Elongational Properties of Polymer Melts for Film Blowing and Thermoforming
,”
Polym. Eng. Sci.
0032-3888,
46
, pp.
1190
1195
.
62.
2008, “
Standard Test for Tensile Properties of Plastics
,”
American Society for Testing and Materials
, Vol.
08
.
01
, Paper No. ASTMD638-08.
63.
Gunel
,
E. M.
, and
Basaran
,
C.
, 2009, “
Micro-Deformation Mechanisms in Thermoformed Alumina Trihydrate Reinforced Poly(Methyl Methacrylate)
,”
Mater. Sci. Eng., A
0921-5093,
523
, pp.
160
172
.
64.
Wang
,
Y.
, and
Adalı
,
T.
, 2002, “
Signal Processing for Magnetic Resonance Imaging and Spectroscopy
,
Stochastic Model Based Image Analysis
,
Marcel Dekker
,
New York
.
65.
Adali
,
T.
, and
Wang
,
Y.
, 2001, “
Multimedia Image and Video Processing
,”
Image Analysis and Graphics for Multimedia Presentation
,
CRC
,
Boca Raton, FL
.
66.
Adali
,
T.
,
Wang
,
Y.
, and
Li
,
H.
, 2002, “
Applications of Neural Networks to Biomedical Image Processing
,”
Handbook of Neural Network Signal Processing
,
CRC
,
Boca Raton, FL
.
67.
Stephens
,
M. A.
, 1974, “
EDF Statistics for Goodness of Fit and Some Comparisons
,”
J. Am. Stat. Assoc.
0162-1459,
69
(
347
), pp.
730
737
.
68.
Goh
,
T. N.
,
Xie
,
M.
, and
Tang
,
X. Y.
, 2006, “
Six Sigma: Advanced Tools for Black Belts and Master Black Belts
,”
Data Transformation for Geometrically Distributed Quality Characteristics
,
Wiley
,
New York
.
You do not currently have access to this content.